{"product_id":"gbt1685-2-2019","title":"GB\/T 1685.2-2019 English PDF (GB\/T1685.2-2019)","description":"\u003ch1\u003eGB\/T 1685.2-2019: Rubber, vulcanized or thermoplastic -- Determination of stress relaxation in compression -- Part 2: Testing with temperature cycling\u003c\/h1\u003e\u003cb style=\"font-size:16px;\"\u003eDelivery:\u003c\/b\u003e 9 seconds. Download (and Email) true-PDF + Invoice.\u003cbr\u003e\u003cb style=\"font-size:16px;\"\u003eGet Quotation:\u003c\/b\u003e Click \u003ca style=\"color: blue;\" href=\"https:\/\/www.chinesestandard.net\/Cart\/Cart.aspx?GB\/T%201685.2-2019_English\" rel=\"nofollow\"\u003eGB\/T 1685.2-2019\u003c\/a\u003e (Self-service in 1-minute)\u003cbr\u003e\u003cb style=\"font-size:16px;\"\u003eNewer \/ historical versions: \u003c\/b\u003e \u003ca style=\"color: blue;\" href=\"https:\/\/www.chinesestandard.net\/PDF.aspx\/GBT1685.2-2019\"\u003eGB\/T 1685.2-2019\u003c\/a\u003e\u003ch2\u003ePreview True-PDF\u003c\/h2\u003e\u003ciframe src=\"https:\/\/www.chinesestandard.net\/Preview_PDF.aspx\/GBT1685.2-2019\" width=\"445\" height=\"600\" title=\"GB\/T 1685.2-2019 True-PDF\"\u003e\u003c\/iframe\u003e \u003cbr\u003e\u003ch2\u003eScope\u003c\/h2\u003eThis Part of GB\/T 1685 specifies two methods for determining the decrease in \u003cbr\u003ecompressive force of vulcanized or thermoplastic rubber, that has been compressed to \u003cbr\u003eand maintained at a constant strain, under temperature cycling conditions. \u003cbr\u003eMethod A. The test temperature alternates between high and low temperatures at set \u003cbr\u003eintervals; the rubber material's aging resistance is evaluated at the high-temperature \u003cbr\u003ephase, while its sealing performance is evaluated at the low-temperature phase. \u003cbr\u003eMethod B. The test temperature alternates continuously between high and low \u003cbr\u003etemperatures, to induce internal thermal stress within the rubber material. \u003cbr\u003eThe compressive force is measured, using a continuous monitoring system. \u003cbr\u003eSpecimens may be cylindrical or annular (ring-shaped). Results vary depending on the \u003cbr\u003edifferent shape and size of the specimens; test results are comparable only when \u003cbr\u003eobtained from specimens of the same shape and size. \u003cbr\u003eAnnular specimens are particularly suitable for determining stress relaxation in liquid \u003cbr\u003eenvironments. \u003cbr\u003e\u003cbr\u003e\u003ch2\u003eBasic Data\u003c\/h2\u003e\u003ctable id=\"TableTabAbout0\" rules=\"all\" border=\"1\" style=\"font-family:Arial;font-size:Small;\"\u003e  \u003ctr id=\"TableTabRow10\"\u003e     \u003ctd id=\"TableTabCell110\" align=\"center\" font=\"bold\"\u003e \u003cb\u003eStandard ID\u003c\/b\u003e \u003c\/td\u003e    \u003ctd id=\"TableTabCell120\" align=\"center\"\u003e GB\/T 1685.2-2019 (GB\/T1685.2-2019)\u003c\/td\u003e  \u003c\/tr\u003e\n\u003ctr id=\"TableTabRow20\"\u003e     \u003ctd id=\"TableTabCell210\" align=\"center\" font=\"bold\"\u003e \u003cb\u003eDescription (Translated English)\u003c\/b\u003e \u003c\/td\u003e    \u003ctd id=\"TableTabCell220\" align=\"center\"\u003e Rubber, vulcanized or thermoplastic -- Determination of stress relaxation in compression -- Part 2: Testing with temperature cycling\u003c\/td\u003e  \u003c\/tr\u003e\n\u003ctr id=\"TableTabRow30\"\u003e     \u003ctd id=\"TableTabCell310\" align=\"center\" font=\"bold\"\u003e \u003cb\u003eSector \/ Industry\u003c\/b\u003e \u003c\/td\u003e    \u003ctd id=\"TableTabCell320\" align=\"center\"\u003e National Standard (Recommended)\u003c\/td\u003e  \u003c\/tr\u003e\n\u003ctr id=\"TableTabRow40\"\u003e     \u003ctd id=\"TableTabCell410\" align=\"center\" font=\"bold\"\u003e \u003cb\u003eClassification of Chinese Standard\u003c\/b\u003e \u003c\/td\u003e    \u003ctd id=\"TableTabCell420\" align=\"center\"\u003e G40\u003c\/td\u003e  \u003c\/tr\u003e\n\u003ctr id=\"TableTabRow50\"\u003e     \u003ctd id=\"TableTabCell510\" align=\"center\" font=\"bold\"\u003e \u003cb\u003eClassification of International Standard\u003c\/b\u003e \u003c\/td\u003e    \u003ctd id=\"TableTabCell520\" align=\"center\"\u003e 83.060\u003c\/td\u003e  \u003c\/tr\u003e\n\u003ctr id=\"TableTabRow60\"\u003e     \u003ctd id=\"TableTabCell610\" align=\"center\" font=\"bold\"\u003e \u003cb\u003eWord Count Estimation\u003c\/b\u003e \u003c\/td\u003e    \u003ctd id=\"TableTabCell620\" align=\"center\"\u003e 14,164\u003c\/td\u003e  \u003c\/tr\u003e\n\u003ctr id=\"TableTabRow70\"\u003e     \u003ctd id=\"TableTabCell710\" align=\"center\" font=\"bold\"\u003e \u003cb\u003eDate of Issue\u003c\/b\u003e \u003c\/td\u003e    \u003ctd id=\"TableTabCell720\" align=\"center\"\u003e 2019-12-10\u003c\/td\u003e  \u003c\/tr\u003e\n\u003ctr id=\"TableTabRow80\"\u003e     \u003ctd id=\"TableTabCell810\" align=\"center\" font=\"bold\"\u003e \u003cb\u003eDate of Implementation\u003c\/b\u003e \u003c\/td\u003e    \u003ctd id=\"TableTabCell820\" align=\"center\"\u003e 2020-11-01\u003c\/td\u003e  \u003c\/tr\u003e\n\u003ctr id=\"TableTabRow90\"\u003e     \u003ctd id=\"TableTabCell910\" align=\"center\" font=\"bold\"\u003e \u003cb\u003eIssuing agency(ies)\u003c\/b\u003e \u003c\/td\u003e    \u003ctd id=\"TableTabCell920\" align=\"center\"\u003e State Administration for Market Regulation, China National Standardization Administration\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003c\/table\u003e\u003cbr\u003e\u003cbr\u003e","brand":"www.ChineseStandard.us -- Field Test Asia Pte. Ltd.","offers":[{"title":"Default Title","offer_id":53657127092538,"sku":null,"price":230.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0821\/5737\/1706\/files\/GBT1685.2-2019EN.1.jpg?v=1782642530","url":"https:\/\/www.chinesestandard.us\/products\/gbt1685-2-2019","provider":"www.ChineseStandard.us (www.ChineseStandard.net)","version":"1.0","type":"link"}